Thermal treatment of pine wood was carried out at 80, 120, 160, and 200 °C for 2, 4, and 6 hours. The highest mean values were, for specific gravity (0.492), moisture content (29.1%), and maximum moisture content (191%), whereas the lowest mean values were for specific gravity (0.418), moisture content (1.20%), and maximum moisture content (127%). The maximum mean values were for shrinkage in longitudinal plane (0.42%), radial plane (4.63%), volumetric shrinkage (9.28%), and maximum mean value tangential plane (3.67%). The minimum mean values were for shrinkage in longitudinal plane (0.04%), radial plane (2.22%), tangential plane (1.55%), and volumetric shrinkage (4.88%). Maximum mean values were for swelling in longitudinal (0.41%), radial (5.22%), and tangential plane (3.15%) and maximum mean volumetric swelling (7.71%), while minimum mean values were for swelling in longitudinal plane (0.08%), radial plane (2.26%), and tangential plane (1.29%) and minimum mean volumetric swelling (3.15%). The highest mean values were for tensile strength (57.3 MPa) and compression parallel to the grain (50.3 MPa), the maximum mean value of bending strength (84 MPa) and compression strength perpendicular to grain (27 MPa), whereas the lowest values were for tensile strength (42.7 MPa), bending strength (7.33 MPa), compression parallel to the grain (7.33 MPa) and compression strength perpendicular to grain (12.3 MPa).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.