This article presents the performance of the short-term bearing capacity on soft clay soil treated by Kenaf geotextile under vertical loading via a small-scale modelling test at unit gravity. The ground model was formulated by consolidating kaolin in a rigid testing compartment. In the loading test, the strip footing was represented by a rigid footing. For the treated case, a series of tests were performed to examine the effects of the burial depth of the Kenaf geotextile on the bearing capacity of the soft soil. The Kenaf geotextile was laid beneath the rigid footing (at the ground surface) and at 50, 75 and 100 mm depth from the soil surface. All the measured results of the Kenaf geotextile treated ground were compared with the untreated ground. The incorporation of Kenaf fibre geotextile was observed to enhance the bearing capacity of soft cohesive clay up to 281% depending upon the depth of the installed geotextile. The geotextile at the surface provided the highest bearing capacity and sustained the highest displacement at failure. The outcome of this research will promote the use of natural fibre geotextiles as sustainable earth reinforcement in temporary earthwork applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.