Abstract
XPS spectra of a spin-coated film poly(vinyl chloride)(PVC) were collected over a period of 243 min at 303 K to determine specimen damage during long exposures to monochromatic Al Kα x-rays. For this PVC film we measured the loss of chlorine as a function of time by rastering a focused 104.6 W, 100 μm diameter x-ray beam over a 1.4 mm × 0.2 mm area on the sample.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.