Abstract
Differential scanning calorimetry (DSC) was used to characterize barium titanate formed after decomposition of barium titanyl oxalate. Three different methods of the oxalate precipitation reaction were used to prepare barium titanyl oxalate which after calcinations result in barium titanates with different barium to titanium ratio ( A/ B). It appears that two factors have effect on Curie temperature: barium to titanium ratio and mechanical stress introduced by milling.