We investigated the thermoelectric properties of Ba8Al16Si30 clathrate samples prepared by combining arc melting and spark plasma sintering methods under two different arc melting conditions. The x-ray diffraction, scanning electron microscopy, and energy dispersive analysis of x-ray studies indicate that Al composition is close to 15, which is higher than that of a single crystal reported, for both arc melting conditions. The carrier concentration of samples decreases to about 1×1021 cm-3, which is lower than reported values so far in Ba8Al16Si30 system. The Seebeck coefficient and the electrical conductivity alter slightly with the arc melting condition due to the slight difference in the carrier concentration. The lattice thermal conductivity (RT) is as low as about 1.3 Wm-1K-1, which is comparable to Bi2Te3-based bulk alloy, independently of the arc melting condition. The thermoelectric figure of merit ZT is about 0.4 at 900 K. An estimation indicates that ZT reaches 0.8 (1200 K) at the optimum carrier concentration of about 3×1020 cm-3 in Ba8Al16Si30 system.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.