Marked ball grinding tests were carried out in the laboratory with a lead-zinc sulphide ore under different experimental conditions using high carbon low alloy steel (cast and forged) and high chrome cast iron balls. Relative ball wear as a function of grinding period and milling conditions was evaluated for the different types of ball materials. The role of corrosion and abrasion-erosion in the wear of grinding media is brought out. Methods to minimise ball wear through control of mill atmosphere and addition of reagents are discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.