Abstract

The effects of axial strains ε a on the critical current of Bi-2223/Ag and Bi-2223/AgMn tapes produced by the powder-in-tube method have been studied at 77 K. The normalized critical current I cn vs axial strain ε a curves I cn( ε a), and its empirical formulae as I cn=1−( ε a/ a) b , where a and b are constants, have been obtained. The critical current degrades more rapidly under large axial tensile strains than under axial compressive strain. The irreversible strain limit of 19-filament, 37-filament Bi-2223/Ag and 61-filament Bi-2223/AgMn superconducting tapes are 0.23–51%, 0.30–36% and 0.43–0.54%, respectively. Strain rate has influence on the irreversible strain limit. The whole I cn( ε a) curve is divided into four ranges: compressive strain regime, first tensile strain regime, second tensile strain regime, third tensile strain regime.