Iron Fischer–Tropsch (F–T) catalyst particles break-up during reaction in slurry phase reactors by physical attrition, and due to chemical stresses caused by phase transformations. Although “chemical” attrition is known to be important with iron (Fe) F–T catalysts, there have been no studies of attrition properties of precipitated Fe catalysts under reaction conditions. Here we report on attrition properties of three precipitated Fe catalysts (100 Fe/3–5 Cu/4–6 K/16–25 SiO2) during F–T synthesis in a stirred tank slurry reactor (STSR). Our results show that after 295–497 h of F–T synthesis with these three catalysts in the STSR, the particle size reduction by fracture was moderate, whereas erosion (generation of particles smaller than 10 μm) was small (2.3–2.7). The attrition strength of these catalysts is adequate for use in Slurry bubble column reactors (SBCRs) for F–T synthesis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.