Abstract

ABSTRACTAnalyzing the attrition of Victorian brown coal during air and steam fluidized bed drying, the change in particle size distribution over a range of initial moisture contents (60% to 0%) and residence times (0 to 60 minutes) was determined. Dried at a temperature of 130°C with a fluidization velocity 0.55 m/s and an initial particle size of 0.5–1.2 mm, both fluidization mediums show a shift in the particle size distribution between three and four minutes of fluidization, with a decrease in mean particle size from 665 µm to around 560 µm. Using differential scanning calorimetry (DSC), the change in particle size has been attributed to the transition between bulk and non-freezable water (approximately 55% moisture loss) and can be linked to the removal of adhesion water, but not to fluidization effects. This is proved through the comparison of air fluidized bed drying, steam fluidized bed drying, and fixed bed drying—the fixed bed drying is being used to determine the particle size distribution as a function of drying. The results show the three drying methods produce similar particle size distributions, indicating that both fluidization and fluidization medium have no impact upon the particle size distribution at short residence times around ten minutes. The cumulative particle size distribution for air and steam fluidized bed dried coal has been modeled using the equation Pd = A2 + (A1 − A2)/(1 + (d/x0)p), with the resultant equations predicting the effects of moisture content on the particle size distribution. Analyzing the effect of longer residence times of 30 and 60 minutes, the particle size distribution for steam fluidized bed dried coal remains the same, while air fluidized bed dried coal has a greater proportion of smaller particles.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call