Abstract
Vanadium oxides may offer high pseudocapacitance but limited electrical conductivity and specific surface area. Atomic layer deposition allowed uniform deposition of smooth nanostructured vanadium oxide coatings on the surface of multi-walled carbon nanotube (MWCNT) electrodes, thus offering a novel route for the formation of binder-free flexible composite electrode fabric for supercapacitor applications with large thickness, controlled porosity, greatly improved electrical conductivity and cycle stability. Electrochemical measurements revealed stable performance of the selected MWCNT–vanadium oxide electrodes and remarkable capacitance of up to ∼1550 F g−1 per active mass of the vanadium oxide and up to ∼600 F g−1 per mass of the composite electrode, significantly exceeding specific capacitance of commercially used activated carbons (100–150 F g−1). Electrochemical performance of the oxide layers was found to strongly depend on the coating thickness.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Energy & Environmental Science
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.