Abstract
The synthesis and characterization of crystalline tungsten disulphide (WS2) solid lubricant thin films grown by atomic layer deposition (ALD) using WF6 and H2S gas precursors was studied. A new catalytic route was established to promote nucleation and growth of WS2 films on silicon surfaces with native oxide. Scanning electron microscopy with energy dispersive spectroscopy and Raman spectroscopy were used to determine the film morphology, composition, and crystallinity. The films exhibited solid lubricating behavior with a steady-state friction coefficient of 0.04 in a dry nitrogen environment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.