Abstract
Ruthenium (Ru) thin films were grown on thermally-grown SiO2 substrates by plasma enhanced atomic layer deposition (PEALD) using a sequential supply of a new betadiketonate Ru metallorganic precursor, dicarbonyl-bis(5-methyl-2,4-hexanediketonato) Ru(II) (C16H22O6Ru) with a high vapor pressure and NH3 plasma as a reactant at the substrate temperature ranging from 175 and 310 degrees C. A self-limited film growth was confirmed at the deposition temperature of 225 degrees C and the growth rate was 0.063 nm/cycle on the SiO2 substrate with very short number of incubation cycles (approximately 10 cycles). The resistivity of PEALD-Ru films was dependent on the microstructural features characterized by grain size and crystallinity, which could be controlled by varying the deposition temperature. Ru film with the resistivity of -20 μΩ-cm and high density of 11.5 g/cm3 was obtained at the deposition temperature as low as 225 degrees C. It formed polycrystalline structure with hexagonal-close-packed phase that was confirmed by X-ray diffractometry and transmission electronic microscopy analysis. Step coverage of PEALD-Ru film deposited with the optimum condition was good (-75%) at the very small-sized trench (aspect ratio: -4.5 and the top opening size of 25 nm).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.