Abstract
A novel catalyst design for electrochemical promotion of catalysis (EPOC) is proposed which overcomes the main bottlenecks that limit EPOC commercialization, i.e., the low dispersion and small surface area of metal catalysts. We have increased the surface area by using a porous composite electrode backbone made of (La0.8Sr0.2)0.95MnO3-δ/Ce0.9Gd0.1O1.95 (LSM/GDC). Highly dispersed Pt nanoparticles with an average diameter of 6.5nm have been deposited on LSM/GDC by atomic layer deposition (ALD). This novel design offers, for the first time, a controllable and reproducible method for the fabrication of EPOC catalysts. The bare electrode backbone shows negligible activity for propane oxidation, while in the presence of Pt nanoparticles a high catalytic activity is obtained above 200°C. The performance of the Pt-loaded LSM/GDC catalyst was significantly improved by application of small currents (I<500μΑ), leading to a 27–33% increase as a function of the open circuit catalytic rate, with apparent Faradaic efficiency values ranging from 1000 to 3860% at 300°C. Our results demonstrate that EPOC is a valid approach for enhancing the catalytic activity of nano-structured catalysts.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have