Abstract
In this work, atomic layer deposition (ALD) has been employed to prepare high-mobility H-doped zinc oxide (ZnO:H) films. Hydrogen doping was achieved by interleaving the ZnO ALD cycles with H2 plasma treatments. It has been shown that doping with H2 plasma offers key advantages over traditional doping by Al and B, and enables a high mobility value up to 47cm2/Vs and a resistivity of 1.8 mΩcm. By proper choice of a deposition regime where there is a strong competition between film growth and film etching by the H2 plasma treatment, a strongly enhanced grain size and hence increased carrier mobility with respect to undoped ZnO can be obtained. The successful incorporation of a significant amount of H from the H2 plasma has been demonstrated, and insights into the mobility-limiting scatter mechanisms have been obtained from temperature-dependent Hall measurements. A comparison with conventional TCOs has been made in terms of optoelectronic properties, and it has been shown that high-mobility ZnO:H has potential for use in various configurations of silicon heterojunction solar cells and silicon-perovskite tandem cells.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.