Abstract
Hafnium oxide (HfOx) films grown by atomic layer deposition (ALD) have recently been demonstrated to provide high‐quality silicon surface passivation. Reports have suggested that changing the composition of the hafnium‐containing precursor can enable films of both charge polarities to be produced. Herein, the passivation quality of hafnium oxide grown with metal amide precursors and a tetrakis(ethylmethylamido)hafnium (TEMAHf) precursor is examined, considering film charge polarity, chemical‐ and field‐based passivation effects, and film crystallinity. Throughout, the properties of TEMAHf‐HfOx are benchmarked against that of hafnium oxide grown with a tetrakis(dimethylamido)hafnium precursor. It is found that precursor choice has no influence on the fixed negative charge polarity (of order −1012 q cm−2) of HfOx films grown via plasma‐enhanced ALD. TEMAHf‐HfOx passivation is influenced by post‐deposition annealing temperature and can passivate with a surface recombination velocity ≤3 cm s−1 on n‐type silicon, compared to surface recombination velocities ≤11 cm s−1 for TDMAHf‐HfOx of a similar thickness.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: physica status solidi (RRL) – Rapid Research Letters
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.