Abstract
Atomic layer deposition (ALD) was used to deposit TiO2 anode material on high surface area graphene (reduced graphene oxide) sheets for Li-ion batteries. An Al2O3 ALD ultrathin layer was used as an adhesion layer for conformal deposition of the TiO2 ALD films at 120 ° C onto the conducting graphene sheets. The TiO2 ALD films on the Al2O3 ALD adhesion layer were nearly amorphous and conformal to the graphene sheets. These nanoscale TiO2 coatings minimized the effect of the low diffusion coefficient of lithium ions in bulk TiO2. The TiO2 ALD films exhibited stable capacities of ∼120 mAh g−1 and ∼100 mAh g−1 at high cycling rates of 1 A g−1 and 2 A g−1, respectively. The TiO2 ALD films also displayed excellent cycling stability with ∼95% of the initial capacity remaining after 500 cycles. These results illustrate that ALD can provide a useful method to deposit electrode materials on high surface area substrates for Li-ion batteries.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.