Abstract
The following study presents a novel approach that utilizes residual stresses inside a component to produce stress-oriented precipitation and achieves texture strengthening during the ageing treatment. Refined investigations for the stress-oriented precipitation of γ″ were achieved via transmission electron microscopes (TEM) and neutron diffraction (ND). The results showed that all three variants of γ″ nucleated at short ageing times. The orienting effect of stress was appreciable only during the Ostwald ripening, due to the change of the γ″/γ lattice mismatch. The effect that the stress-oriented precipitation had on the mechanical properties was evaluated and analyzed via tensile tests.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.