Abstract
ABSTRACT Fluxes are added to steelmaking process to form basic slag and limit refractory lining consumption. Early formation of CaO- and MgO-saturated slag is critical for process productivity. To achieve this, flux must be dissolved in the melt in a limited process time, and the properties of a slag additive influence the fluxing efficiency. The dissolution behavior of samples with different qualities (i.e. raw dolomite, limestone, soft-burnt and hard-burnt quicklime and dolime) was investigated in the pre-melted model BOF and EAF slags at 1673 K and 1723 K. The disc-shaped sample was immersed into the melt and left there until slag solidification was reached. After a holding time between 5 and 20 minutes, the crucible with the sample were quenched with liquid nitrogen. The fused samples were analyzed by SEM method. Based on comparison of slag morphology and concentration changes in the slag, the dissolution behavior of the samples was examined.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.