Abstract
This paper presents a model for assessing primary water stress corrosion cracking (PWSCC) damage to pressurized water reactor (PWR) steam generator tubes. PWSCC damage has been detected at three locations in the recirculating steam generator: expansion transition regions, U-bends, and tube dents. The model accounts for residual stresses, microstructure, and primary coolant temperatures. High residual tensile stresses and low mill-annealing temperatures contribute significantly to PWSCC. PWSCC is a thermally activated process; small increases in operating temperature accelerate damage. The model employs a Weibull distribution to represent tube degradation results obtained from inservice inspections and from destructive examinations. The model can be used to estimate the times to steam generator tube failures caused by PWSCC. This paper also evaluates remedial measures for PWSCC damage and presents a procedure for life assessment of steam generator tubes.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.