A non-destructive assessment of Zircaloy-2 samples charged with hydrogen in the range of 50 to 1150 mg/kg has been made using ultrasonic and eddy current testing. It has been found that the ratio of the longitudinal to the shear wave velocity is a parameter which can be directly correlated with the hydrogen content up to a level of 100 to 200 mg/kg. This parameter together with the values of longitudinal and shear wave velocities can be utilized in a multi-parametric correlation approach for estimation of higher levels of the hydrogen content (up to 1150 mg/kg). The sensitivity at different ranges has been found to be acceptable. Ultrasonic attenuation measurements at higher frequencies and eddy current test parameter are also effective for estimation of hydrogen levels above 250 mg/kg in zirconium alloys. Microstructural characterization including TEM studies have been carried out for studying the influence of the type and the morphology of hydride precipitates on ultrasonic parameters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.