This study evaluated the fluoride release of alkasite restorative material (ARM) and giomer penetrating the dentin adhesive layer. Twenty specimens were prepared for each restorative material, and dentin adhesive with uniform thickness was applied to half of them. The prepared specimens were placed in a polyethylene tube containing 2.0 mL of deionized water and deposited in a 37.0°C water bath for the study duration. The amount of fluoride release was measured on the 1st, 3rd, 7th, 14th, 21st, and 28th days after deposition. The dentin adhesive applied to the ARM and giomer could not completely block the fluoride release; however, it significantly reduced its amount. The cumulative amount of fluoride release of the ARM after 28 days was higher than that of the giomer regardless of the application of dentin adhesive.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.