Abstract

In this study, short-term accelerated creep tests were conducted using the stepped isostress method (SSM) to investigate the impact of hydrothermal treatment on the long-term creep behaviour of Japanese cedar wood and to determine optimal hydrothermal treatment conditions. The results showed that SSM can effectively predict the creep behaviour of hydrothermally treated wood. Among the treatment conditions tested, Japanese cedar wood treated hydrothermally at 180 °C for 4 h exhibited higher flexural strength retention (91%) and moisture excluding efficiency (MEE) (44%) and demonstrated superior creep resistance compared to untreated wood. When subjected to a 30% average breaking load (ABL) over 20 years, the specimen's creep compliance, instantaneous creep compliance, b value, activation volume, and improvement in creep resistance (ICR) were 0.17 GPa-1, 0.139 GPa-1, 0.15, 1.619 nm3, and 4%, respectively. The results indicate that subjecting Japanese cedar wood to hydrothermal treatment at 180 °C for 4 h has a negligible effect on its flexural properties but results in significant improvements in both dimensional stability and creep resistance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.