Abstract

This study evaluated bond strength of glass fiber posts to root dentin using push-out (PO) and diametral compression (DC), testing glycolic acid as a conditioner and varying dentin moisture. An additional aim was to test whether DC can be an alternative test to PO for bond strength assessment. Eighty bovine teeth were divided into eight groups (n=10) defined by the use of either 37% glycolic acid or 37% phosphoric acid (PA) on moist or wet dentin before bonding with either Adapter SingleBond/RelyX ARC or One Step Plus/Duo-Link Bisco. Each tooth provided discs with an internal diameter of 2mm, external diameter of 5mm, and height of 2mm, which underwent PO and DC. Finite element analysis (FEA) was carried out on 3D models. When analyzing PO results through linear regression, the highest values of bond strength were observed using glycolic acid on wet dentin in the cervical and middle thirds of the teeth. Analyzing DC results, the only statistical influence on values was the dental thirds. The scatterplot of the DC results and the PO bond strength values indicated no relationship between the results of the two tests (r=0.03; p=0.64). PO test detected more sensitive changes in bond strength values than DC.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.