Abstract

Application-oriented characterizations were carried out for Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ permanent magnets in which both high temperature effects and aging effects are taken into account. Experimental results indicate that application-oriented characterization may provide data more application-oriented than traditional high temperature aging test data. The irreversible loss of the maximum energy product of Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ caused from thermal demagnetization increases rapidly with temperature. It should be possible to reduce this loss by optimizing magnet compositions and heat treatments, which would significantly improve the high temperature performance of Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ magnets.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.