With the development of modern building design and construction technology, high strength concrete technology were getting more use in engineering and more requirements. The authors produced C80 HPC by using Portland cement, blast furnace slag, micro bead and Flyash as cementitious material, have prepared the concrete with grade of C80, low pumping resistance (rewinding time less than 6s), low shrink (72h early self-shrinkage value at 0.028%), high workability (slumps over 240mm and divergence over 700mm) and high durability (diffusion coefficient in concrete after 28d was 1.35×10-12 m2/s), which would match the requirements of the Guangzhou East Tower.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.