Abstract

A polysilicon sealed pad oxide local oxidation process has been investigated. The oxidation mask in this method has a polysilicon frame formed along the perimeter of a conventional mask pattern by a self-aligned technique. This technology is completely free of “bird's beak” formation which is particularly important for increasing the packing density.