Abstract

The results of an experimental analysis of the effect of the volume content of voids in the range of 0.25–5% on the crack resistance of structural carbon plastics are presented. To obtain a variation of the volume content of voids, samples were manufactured using the vacuum-infusion method with variations in the vacuum strength from –760 to –150 mm Hg. The total volume content of voids was determined by methods of optoacoustic structuroscopy, scanning electron microscopy, and chemical etching to obtain comparative data. The experimental dependences of the characteristics of the interlaminar crack resistance on the volume content of voids under static and cyclic loading of samples in the normal-separation mode were obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.