Abstract
Here Analytical Hierarchical Process (AHP) was used for optimization of weld strength of Al-8%SiC composite using Pulsed Current Tungsten Inert Gas (PCTIG) welding. The experiment was designed using Taguchi L9 OA. The parameters used as criteria were pulse on time, pulse frequency, peak current, base current, peak temperature and cooling rate. The optimum condition were at peak current of 160A, base current of 60A, pulse on time of 50%, pulse frequency of 5Hz and optimum values of peak temperature and cooling rate were 446°C/s and 20°C/s respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.