Abstract

The Mn atom in the cubic polymorph of CeMnNi(4) appears to be located in an oversized cage-like structure, and anomalously large atomic displacement parameters (ADPs) for the Mn atom indicate that it is a potential "rattler" atom. Here, multitemperature synchrotron powder X-ray diffraction data measured between 110 and 900 K are used to estimate ADPs for the Mn "guest" atom and the "host" structure atoms in cubic CeMnNi(4). The ADPs are subsequently fitted with Debye and Einstein models, giving Θ(D) = 301(2) K for the "host" structure and Θ(E) = 165(2) K for the Mn atom. This is higher than typical Einstein temperatures for rattlers in thermoelectric skutterudites and clathrates (Θ(E) = 50-80 K), indicating that the Mn atom in cubic CeMnNi(4) is more strongly bonded. In order to probe the chemical interactions of the potential Mn rattler atom, atomic Hirshfeld surface (AHS) analysis is carried out and compared with AHS analysis of well-established guest atom rattlers in archetypical skutterudites, MCoSb(3). Surprisingly, the skutterudite rattlers have more deformed AHSs than the Mn atom in cubic CeMnNi(4). This is related to the highly ionic nature of the skutterudite rattlers, which is not taken into account in the neutral spherical atom approach of the AHS. Additionally, visualization of void spaces in the two materials using the procrystal electron density shows that while the Mn atom is tightly fitting in the CeMnNi(4) structure then the La atom in the skutterudite is truly situated in an oversized cage of the host structure. Overall, we conclude that the Mn atom in cubic CeMnNi(4) cannot be coined a rattler.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.