Abstract

The objective of this study was to assess AISI 4340 and 300 M steels electropolishing performance in a concentrated perchloric/acetic acid electrolyte. The statistical analysis on a two-level fractional design (FFD) 24-1 was proposed to define an adequate tool to describe the dissolved thickness and the final surface via arithmetic roughness Ra. A compromise zone was defined for each steel by considering all the requirements for both responses of each steel: dissolved thickness between 15–17 μm and arithmetic roughness criteria less than 0.06 μm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.