A method of manufacturing optical coatings for germanium optics used at terahertz frequencies has been developed. The various optical coatings used at terahertz frequencies are difficult to manufacture conventionally because these coatings must be as thick as several tens of micrometers, which is far thicker than those used in the optical region. One way to overcome this problem is to form a silicon oxide layer through plasma-enhanced chemical-vapor deposition, with silane (SiH4) as a source gas. Using this method, I formed 21-microm-thick silicon oxide films as antireflection (AR) layers for germanium optics and obtained low reflection at 1.7 THz (wavelength, lambda = 175 microm). This method is easily applied to large-aperture optics and micro-optics as well as to optics with a complex surface form. The AR coatings can also be formed for photoconductive detectors made from germanium doped with gallium at a low temperature (160 degrees C); this low temperature ensures that the doped impurities in the germanium do not diffuse. Fabrication of optical coatings upon substrates that have refractive indices of 3.84-11.7 may also be possible by control of the refractive indices of the deposited layers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.