Abstract

Two distinct Tafel regions are observed in the active region of the anodic polarization curve of iron in ammoniacal carbonate solution. A prepassive layer may form in the Tafel region at the higher overpotentials. A hydrogen oxidation peak is proposed to occur in the lower overpotential Tafel region. Anodic dissolution of iron in both Tafel regions is under mixed surface and diffusion control. The passivation of iron in ammoniacal solution involves charge transfer followed by a rate controlling chemical step. The stability and/or thickness of the passive layer and the Fe(III)/Fe(II) ratio increase with more noble potentials in the passive region.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.