Abstract

Well-aligned ZnO nanorod arrays were synthesized by a wet chemical method on the glass substrate with ZnO thin film as seed layer prepared by pulsed laser deposition. The effect of annealing temperature on the luminescence characteristics was investigated. As the annealing temperature increased, the photoluminescence properties show a general enhancing tendency. The nanorod array with high ultraviolet emission and negligible visible light emission (designated by the photoluminescence intensity ratio of ultraviolet to visible emission of 66.4) is obtained by annealing the sample at 700 °C for 1 h. Based on the results of X-ray photoelectron spectroscopy and photoluminescence spectra, the mechanisms of visible emission were discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.