In this work, bulk anisotropic Mn-Al-(C) magnets have been produced by hot-deforming arc-melted alloys. The hot-deformed magnets develop a texture in a plane perpendicular to the deformation direction. Optimum magnetic properties have been obtained in a magnet with nominal composition Mn53.5Al44.5C2 with values of remnant magnetization, coercivity, and energy product of 2.2 kOe, 3.3 kG, and 1.8 MGOe, respectively. A maximum coercivity of 2.8 kOe has been obtained in the magnet with composition Mn54.5Al43.5C2. Addition of C is effective in increasing the coercivity of the substituted alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.