Abstract

AbstractThe isomerization of allyl ether to propenyl ether end group in anionically‐polymerized poly (propylene oxide) was monitored by 1H NMR spectroscopy. It was confirmed that the reaction followed a simple second‐order rate law: −d[allyl]dt = k2[allyl] [O−]. Values of k2 determined over the 90–130°C temperature range, indicated an activation energy of 116 kJ mol−1. © 1994 John Wiley & Sons, Inc.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.