Aggregates occupy ±70% of the concrete volume and their quality must meet specifications. Concrete surfaces submerged in water for a long time cause concrete failure due to the reaction between aggregate and cement to form silica gel. The wear value of granite is less than gravel, so this study used granite as a substitute for coarse aggregate. This study was conducted to assess the resistance of SCC concrete with 0%, 25%, and 30% granite stone variations to alkali-silica reaction attack. The experimental method was applied to the study with ACI method mix design as well as 25 MPa plan fc'. Concrete cylinder samples 150 mm x 300 mm aged 28 days were used in the compressive strength test, alkali-silica reaction expansion test used mortar block samples 285 mm x 25 mm x 25 mm in 80±2˚C NaOH solution bath for 14 days. The optimum compressive strength of 32.17 MPa and the lowest percentage change in length of 0.04% was obtained by sample BG.25-SCC, indicating that granite stone is not reactive to silica alkali reaction because the percentage change in length <0.10%. This study concludes that granite stone can improve the resistance of concrete to silica alkali reaction.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call