Abstract
In the present work, the role of the optically inactive co-dopant magnesium in increasing the emission intensity of Zn2SiO4:Mn2+ has been established. It is shown that the dominant reasons for the increase in green luminescence intensity are the enhancement in the prohibition of the 4T2(4G) → 6A1(6S) transition and the decrease in non-radiative dissipation of absorbed excitation energy upon the introduction of Mg2+ ions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.