Paper is focused on analysis of a local shrinkage and injection pressure of the biodegradable materials PLLA and PLA. Analysed products were prepared with thickness of 4 mm in the patent injection mould. The technological parameters of the injection moulding were established by the Taguchi method. In this article, the influence of these main technological parameters on the local shrinkage and injection pressure is evaluated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.