Abstract
The development of the teak wood processing industry is growing rapidly, especially in the Aceh area. Allows a lot of waste to be generated. This research was conducted by utilizing sawn wood waste into particle boards. To test the physical and mechanical properties of particleboard using a matrix of teak waste and SHCP 2668 WNC resin with a ratio of 60: 40, and variations in treatment (NaOH) 2,5, 5, and 7,5% in immersion for 2 hours. Then the particleboard is compressed using a hot press machine at a temperature of 150˚C for 20 minutes, and a pressure of 50 kg/cm2. Then tested according to SNI 03-2105-2006 standards, namely density, thickness expansion, moisture content, elasticity, and modulus of fracture. The results of the particle board test on the physical and mechanical properties test, namely the density yielded the best value for the 5% (NaOH) treatment with a value of 0.854 gr/cm3, the best water content test with 2.5% (NaOH) treatment with a value of 4.563 %, viscous development with treatment (NaOH) 5% with a value of 7.573%, the best elasticity test on treatment (NaOH) 2.5% with a value of 2.470 kgf/cm2, and the best fracture modulus test on treatment (NaOH) 7.5% with a value of 48.611 kgf/cm2 declared to meet the standard requirements of SNI 03-2105-2006. With alkaline treatment, particleboard gives a relatively good value compared to no treatment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Engineering, Science and Information Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.