AbstractThis work is focused on the analysis, modelling and scale‐up of a process of styrene purification. The first step in synthetic rubber production is to eliminate 4‐tert‐butylcatechol (TBC) which is added to styrene to prevent homopolymerisation during transport and storage. This process is carried out on an industrial scale by means of adsorption onto activated alumina. Equilibrium experiments at 10 °C correlated to the Langmuir–Freundlich equation: with a weighted standard deviation of 3.38%. Fixed bed column experiments were carried out on a laboratory scale to obtain breakthrough curves. A mathematical model that considers film and pore mass transfer resistances described satisfactorily the experimental results with a value of Dp = 3.96 × 10−9 m2 s−1 which was obtained from correlation of experimental data to simulated curves. Finally, a pilot plant was built and operated in order to verify the validity of the mathematical model and parameters obtained previously.© 2002 Society of Chemical Industry

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.