Abstract

Abstract Modern single crystal (SX) turbine blades are fabricated by directional solidification using a grain selector. The grain selection process was investigated by numerical simulation and verified by the experiment. A coupled ProCAST and cellular automaton finite element (CAFE) model was used in this study. According to the latest literature data, we designed the grain selector. Simulation confirmed an optimal grain selection efficiency of the applied selector geometry. The obtained experimental results reveal the possibility of stray grain formation in SX castings with a designed selector, in contrast to the simulation results.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.