Abstract

AbstractCrosslinked styrene‐butadiene and butadiene rubbers can efficiently be analyzed by liquid chromatography and FT‐IR spectroscopy. In a first step the vulcanizate is pyrolyzed under mild conditions. The resulting high molar mass fragments are extracted from the bulk material and analyzed by size exclusion chromatography. The molar masses of the extractables are in the range of 3 000 to 25 000 g/mol. The chemical composition as a function of molar mass is visualized by coupled SEC‐FT‐IR spectroscopy. By quantitative analysis of the FT‐IR spectra the concentrations of the different structural units, including styrene, 1,4‐trans‐butadiene, 1,2‐vinylbutadiene, and 1,4‐cis‐butadiene, are determined. It is shown that the chemical composition of the original non‐crosslinked rubbers and the chemical composition of the extractables are rather identical. Therefore, this technique can be used to obtain structural information on rubber formulations even in the case when the material is already vulcanized.SEC chromatograms of SBR 1712 and the extractables after pyrolysis, stationary phase: SDV linear, mobile phase: THF, detector: ELSD.magnified imageSEC chromatograms of SBR 1712 and the extractables after pyrolysis, stationary phase: SDV linear, mobile phase: THF, detector: ELSD.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.