Abstract

The purpose of this study was to determine the bending strength of the weld in the connection process with Tungsten Inert Gas (TIG) to the 5083 series aluminum (Al) plate 6 mm thick, the welding was carried out with various current strength treatments, namely 130 A, 140 A, 150 A. and Argon gas discharge of 5 lt/minute, 10 lt/minute, 15 lt/minute in each welding process, and also to find out the defects in the weld area after the bending test was carried out. The method used in this study is the analytical method, which is the method used to test by adding different treatments of current and gas discharge variations during the specimen welding process, so that later on we will get a different welding strength difference in each specimen. From the results obtained from the research on this sample, welding using Argon gas discharge which is

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.