Abstract

We reanalyze the effect of silver (Ag2+) and copper (Cu2+) coating solutions for the thickness of the layer on aluminum (Al) materials with increased electrical currents 0.4A, 0.8A, 1A, 1.2A, and 1.4A and increased thickness layer (10µm, 20µm, 30µm, 40µm, and 50µm), as well as the previous study was conducted. We used the electroplating method and thickness test, as well as the Brinell hardness test for both coating solutions. The results show statistically significant (p-value < 0.05, one-tailed) between high electric current and aluminum (Al) coating process with silver (Ag2+) and copper (Cu2+), as well as silver (Ag2+), get the faster coating process time. The Brinell hardness test shows a statistically significant difference (p-value < 0.05, one-tailed) between the high thickness layer and HB value (Ag-coated and Cu-coated).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.