Abstract

The purpose of this paper is to clarify the impact of pitting corrosion and erosion on the directionally solidified (DS) GTD-111 turbine blade behavior. Moreover, the pitting corrosion and oxidation phenomena engendered inside cooling channels of the turbine blade are utterly highlighted. Other features such as the η (Ni3, Ti) platelets nucleation, needle σ-phase precipitation at the interface NiPtAl/(DS) GTD-111 substrate are exhibited as well. Finally, the different microstructural changes in (NiPtAl) coating strata against hot corrosion, oxidation and interaction with (DS) GTD-111 substrate are revealed and argued.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.