Abstract
So far many attempts have been made to synthesize phase-pure Ti3AlC2 MAX-phase. But still the challenge posed by the presence of TiC and Ti-Al based intermetallic transient impurity phases in the final product is a persisting problem. Spark plasma sintering (SPS) technique has been the most successful method to decrease the impurity content of the final product. Even so, synthesis of phase-pure Ti3AlC2 MAX-phase, without any TiC and Ti-Al based intermetallic impurities, has not been achieved and reported in literature with substantial evidences. Further, high purity Ti3AlC2 MAX-phase synthesized using SPS technique has shown lack of phase and microstructural stability above 1350°C temperature. In this work, we have reported an optimized method for producing phase-pure Ti3AlC2 MAX-phase (having more than 99 % purity) using commercial grade Ti, Al and C elemental powders through SPS technique. The final product also showed very good high temperature stability up to 1500°C under flowing Argon inert atmosphere.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.