Abstract

Welding is a fabrication of joining materials into one component. Defects are unavoidable during the welding process, and hence the inspection of welds is a most important task in many industries. In this work, a Computer Aided Detection (CAD) system is designed to detect weld defects based on image processing techniques. It is a non-destructive testing which uses X-ray images. The proposed system mainly consists of three stages; gradient image formation, filtration by Gaussian pyramidal filters algorithm and segmentation by Expectation and Maximization (EM) algorithm. In this study, GD X-ray weld image database is used to evaluate the proposed system. The performance analysis of the proposed system is done by measuring the sensitivity, specificity, and accuracy of the segmented image with the help of its corresponding ground truth images.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.