AbstractLocally sourced red earth (RE) was air‐dried, pulverized, and screened with a sieve of mesh size 75 nm. It was characterized in terms of its moisture content, loss on ignition, silica content, iodine adsorption number, oil absorption, pH, and metal oxide compositions. Natural rubber, standard Nigerian rubber used for this work was first characterized in terms of its dirt, ash and nitrogen contents, volatile matter, plasticity retention index, and Mooney viscosity. The RE was applied as filler wholly and in blends with standard carbon black, CB (N330) filler in the natural rubber compounding using efficient vulcanization system. The cure and the physicomechanical properties of the compounds and vulcanizates were, respectively, measured as function of filler loading. The results were compared with those of the standard carbon black (N330)‐filled natural rubber. It was found, that the RE‐filled natural rubber showed substantial reinforcement of the rubber, though inferior to carbon black (N330) filled vulcanizates, the tensile strength of the carbon black‐filled vulcanizates is about one half times that of the RE‐filled vulcanizates. The tensile properties of the RE‐filled vulcanizates improved markedly by blending the RE‐filler with the carbon black (N330). © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call