Abstract

Present work is an investigation of slurry erosion behavior of WC–CoCr cermet coatings deposited with two different WC grain sizes. HVOF thermal spray process was employed due to its high velocity and low flame temperature characteristics resulting in quality coating. HVOF spraying was assisted with in-flight particle temperature and velocity measurement system to control its heating. Slurry erosion testing was performed using a pot-type slurry erosion tester to evaluate slurry erosion resistance of the coatings. Two parameters were considered for testing viz. erodent particle size and slurry concentration. Surface morphology was examined using SEM images and phase identification was done by XRD. The erosion behavior and mechanism of material removal was studied and discussed based on microstructural examination. It was observed that WC–CoCr cermet coating deposited with fine grain WC exhibits higher slurry erosion resistance under all testing conditions as compared to conventional cermet coating.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.