Abstract

The overall kinetics of the isothermal transformation of austenite to bainite and to pearlite in high-purity Fe-C-3 at. pct X alloys (X = Mn, Si, Ni, or Cu) containing 0.1 wt pct C and 0.4 wt pct C were investigated with quantitative metallography and transmission electron microscopy (TEM) to ascertain the presence or absence of the incomplete reaction phenomenon. The incomplete transformation of austenite to bainite was not observed in the Fe-C-Si, Fe-C-Ni, Fe-C-Cu, or Fe-0.4C-Mn alloys. It was found, however, in the Fe-0.1C-Mn alloy. Transmission electron microscopy results indicate that sympathetic nucleation of ferrite without carbide precipitation is a necessary but not a sufficient condition for the development of the incomplete reaction phenomenon. Transformation resumes following stasis in the low-carbon Fe-C-Mn alloy with the formation of a nodular bainite. The results support the view that the incomplete transformation of austenite to bainite is a characteristic of specific alloying elements and is not an inherent trait of the bainite reaction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.